Butt welding employing fusion. Clean, leak- proof and permanent joints can be
made by following the steps below
Cleanly cut the pipes as required
Remove fibrous material and chamfer inner edges using a rough file.
Bring the cut surfaces together and check alignment
Heat welding mirror to 210-degree C, bring the cut surfaces to be joined into
Contact with mirror. The material will melt.
made by following the steps below
Cleanly cut the pipes as required
Remove fibrous material and chamfer inner edges using a rough file.
Bring the cut surfaces together and check alignment
Heat welding mirror to 210-degree C, bring the cut surfaces to be joined into
Contact with mirror. The material will melt.